Use of thermography to calibrate fusion welding procedures in virtual fabrication applications

D. Camilleri, T.G.F. Gray, T. Comlekci

Research output: Chapter in Book/Report/Conference proceedingChapter

Original languageEnglish
Title of host publicationInfraMation 2004
Number of pages406
Publication statusPublished - 2004

Keywords

  • thermal imaging
  • infrared
  • thermography

Cite this

@inbook{bd7aaa88a94548c188860ffe47cda40e,
title = "Use of thermography to calibrate fusion welding procedures in virtual fabrication applications",
keywords = "thermal imaging, infrared, thermography",
author = "D. Camilleri and T.G.F. Gray and T. Comlekci",
note = "Proceedings of the 2004 Infrared Camera Applications Conference, Las Vegas, USA.",
year = "2004",
language = "English",
booktitle = "InfraMation 2004",

}

Use of thermography to calibrate fusion welding procedures in virtual fabrication applications. / Camilleri, D.; Gray, T.G.F.; Comlekci, T.

InfraMation 2004. 2004.

Research output: Chapter in Book/Report/Conference proceedingChapter

TY - CHAP

T1 - Use of thermography to calibrate fusion welding procedures in virtual fabrication applications

AU - Camilleri, D.

AU - Gray, T.G.F.

AU - Comlekci, T.

N1 - Proceedings of the 2004 Infrared Camera Applications Conference, Las Vegas, USA.

PY - 2004

Y1 - 2004

KW - thermal imaging

KW - infrared

KW - thermography

M3 - Chapter

BT - InfraMation 2004

ER -