Intentional weld defect process: from manufacturing by ‎‎robotic welding machine to inspection ‎using TFM phased ‎‎array ‎

Research output: Chapter in Book/Report/Conference proceedingConference contribution book

3 Citations (Scopus)
34 Downloads (Pure)

Fingerprint Dive into the research topics of 'Intentional weld defect process: from manufacturing by ‎‎robotic welding machine to inspection ‎using TFM phased ‎‎array ‎'. Together they form a unique fingerprint.