Effect of surface machining on intergranular stress corrosion cracking (IGSCC) in sensitised type 304 austenitic stainless steel

S. Rahimi, K. Mehrez, T. J. Marrow

Research output: Contribution to journalArticlepeer-review

15 Citations (Scopus)
276 Downloads (Pure)

Fingerprint

Dive into the research topics of 'Effect of surface machining on intergranular stress corrosion cracking (IGSCC) in sensitised type 304 austenitic stainless steel'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemical Compounds